Sunday, June 6, 2010

Week 8

Just realized that i did not update my week 8 blog.

There is a new term i learnt during week 8 which is 'coplanarity' where when a package is placed flat on a surface table, we can notice there are certain sides of the package which is not touching the table. They are purposely designed that way and not categorized as defects, unless the coplanirity (the height from the surface to the lead legs) exceeded certain numbers. I had the chance to know it when there were customers' complaint on it.

Hopefully i have a chance to ask more details of it in the future. And Friday was Wesak Day off day =D

Wednesday, May 26, 2010

Week 7 in review

Last week, i was doing most of the same thing as last time, doing reject mapping for packages with flashes / mold flashes problems.

But i still able to learn a few new things. Mr.Lee had shown me how to even further use the functions of Profile Projector. I was taught on how to measure the lead foot length and the shank angle to check whether the specification has gone out of range. This is to keep in check to prevent future customers' complaints on bent shoulder, overly bent lead, etc.

Last Friday, i have the opportunity to help out my supervisor and Mr.Lee on one of the emergency call of complaints. Many lots were suspected to have bent shoulder and prevention had to make quickly from the lots shipping out to customers. Finding the appropriate machine with the correct package, i converted much of the data into soft-copy for my supervisors' usage for their meeting.

And also, it's time to begin my final report, everything don't wait until last minute !